Specification Brand : Solderweld BulletPoint : Made in United States BulletPoint1 : Solderweld Part number SW-SS15F1 15% Silver Sil-Sol Brazing Rod Sticks 1 Pound BulletPoint2 : The self fluxing property of this filler metal is effective on copper only. BulletPoint3 : For copper-base alloys, such as brass or bronze, the joints should be fluxed. BulletPoint4 : Should not be used on nickel-base and iron-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints. BulletPoint5 : Should not be used where the joints are exposed to sulfur compounds, especially in gases or oils at temperatures above normal room temperature. Color : Silver ExternallyAssignedProductIdentifier1 : 0859574007041 ExternallyAssignedProductIdentifier2 : 859574007041 ItemName : Solderweld SW-SS15F1 15% Silver Sil-Sol Brazing Rod Flat Sticks 18" Long 1LB ItemPackageDimensions_Height : 1 inches ItemPackageDimensions_Length : 20.25 inches ItemPackageDimensions_Width : 1 centimeters ItemPackageQuantity : 1 ItemTypeKeyword : solder Manufacturer : Solderweld Material : metal ModelName : 3 Piece Silver Solder Sheet ModelNumber : SOLD-0078 NumberOfBoxes : 1 NumberOfItems : 1 PartNumber : SW-SS15F1 ProductDescription : Solderweld Part number SW-SS15F1 15% Silver Sil-Sol Brazing Rod Sticks 1 Pound Developed primarily for use on copper, but its use has extended to other nonferrous copper based alloys. Used extensively on refrigeration units, air conditioning apparatus, electrical conductors, copper and brass fittings and copper to brass equipment. Features: The self fluxing property of this filler metal is effective on copper only. For copper-base alloys, such as brass or bronze, the joints should be fluxed. Should not be used on nickel-base and iron-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints. Should not be used where the joints are exposed to sulfur compounds, especially in gases or oils at temperatures above normal room temperature. Exposure to pressured steam can also result in accelerated corrosion. ProductSiteLaunchDate : 2022-07-22T18:28:01.276Z SafetyDataSheetUrl : https://www.macdermidalpha.com/sites/default/files/sds_pdfs/NA/245ALLOY63_KESTER%20SDS%20GHS%20AMERICAS_ENGLISH%20%28US%29.PDF Size : Set of 4 SupplierDeclaredDgHzRegulation : not_applicable SupplierDeclaredHasProductIdentifierExemption : 1 UnitCount : 1