SpecificationBrand : Solderweld
BulletPoint1 : Solderweld Part number SW-SS1524K Sil Sol 15% Sil-Sol Round Rod 1 Pound Sticks
BulletPoint2 : Round rods with better flow for more effective joints
BulletPoint3 : The self fluxing property of this filler metal is effective on copper only.
BulletPoint4 : For copper-base alloys, such as brass or bronze, the joints should be fluxed.
BulletPoint5 : Should not be used on nickel-base and iron-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints.
ExternallyAssignedProductIdentifier : 00840338553522
ExternallyAssignedProductIdentifier1 : 0859574007270
ExternallyAssignedProductIdentifier2 : 859574007270
ExternallyAssignedProductIdentifier3 : 00652426921584
ItemDisplayWeight : 5 ounces
ItemForm : Rod
ItemName : Solderweld SW-SS1524K15% Silver Sil-Sol Round Brazing Rod 18" Long 1LB Sticks
ItemPackageDimensions_Height : 1 inches
ItemPackageDimensions_Length : 18.5 inches
ItemPackageDimensions_Width : 1 inches
ItemPackageQuantity : 1
ItemShape : Rectangular
ItemTypeKeyword : brazing-rods
Manufacturer : Solderweld
Material : metal
Material1 : Silicone
Material2 : Copper
ModelNumber : SILBRZ-045-10T
NumberOfItems : 1
PartNumber : SW-SS1524K
ProductDescription : Solderweld Part number SW-SS1524K Sil Sol 15% Sil-Sol Round Rod 1 Pound Sticks Developed primarily for use on copper, but its use has extended to other nonferrous copper based alloys. Used extensively on refrigeration units, air conditioning apparatus, electrical conductors, copper and brass fittings and copper to brass equipment. Features:
- Round rods with better flow for more effective joints
- The self fluxing property of this filler metal is effective on copper only.
- For copper-base alloys, such as brass or bronze, the joints should be fluxed.
- Should not be used on nickel-base and iron-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints.
- Should not be used where the joints are exposed to sulfur compounds, especially in gases or oils at temperatures above normal room temperature.
- Exposure to pressured steam can also result in accelerated corrosion.